Ramming Mix
Ramming Mix
Al2O3 % |
35 |
|
Bulk Density g/cm3 |
110°С×16h |
1.7 |
Cold Crushing Strength MPa |
110°С×16h |
10 |
Modulus of Rupture MPa |
110°С×16h |
2.0 |
Linear Change % |
1450°С×3h |
±0.5 |